1.1 This practice covers determination of glass transition temperatures of hydrocarbon (HC) resins by differential scan-ning calorimetry (DSC).
1.2 This practice is applicable to HC resins as defined in Terminology D6640. The normal operating temperature range is from the cryogenic region to approximately 180°C. The temperature range can be extended.